DATA SHEET
DIRECTIONS OF USE
-
Prepare wall surface by scraping off flaked coatings and ensure removal of fungus and algae
growth with suitable biocide treatment.
-
The surface must be free from loose particles, dust and moisture.
-
Take maximum precautions where the water tends to accumulate, i.e places like parapet,
sunshade, etc.
-
The exterior surface must be free from seepage and constant dampness. During
the rainy season, allow 2-3 days of sunshine for surface to dry before starting painting.
-
Newly plastered walls must be allowed to cure for 6 months before painting.
-
To 1 ltr of Ocean Exterior Emulsion add 750 ml of clean portable water. For best results,
apply 2 coats. Between coats, allow minimum of 4 hours gap.
*Actual Coverage may vary from the quoted coverage due to factors such
as method and mode of application and surface roughness and porosity.
COATS
AREA
2 COATS ON
NORMAL MASONARY
SURFACE
55 - 60 Sq.ft/ltr.*
PRECAUTIONS:
-
Do not apply putty or cement primers on exterior walls. Cracks can be filled with white cement or mixture of cement and sand if necessary.
-
Do not over thin the paint. Over dilution of Ocean Acrylic Exterior Emulsion may result in shade variation, poor hiding, poor bonding and flaking.
-
Do not use any universal strainers or other colourants.
TECHNICAL DATA :
Areas of application RCC, Masonary, Asbestos, etc
Viscosity 90-100 krebs unit at 30◦ C Stormer Viscometer
Consistency Smooth & Flowing
Thinner Clean portable water
Mode of application Brush, Roller or Spray
Coverage 55 to 60 sq ft, per kg/ 2 coats ; 45 to 50 sq ft/ltr for coats depending on the porosity and absorbtion of the surface.
Minimum DFT 35-40 Microns
Drying Time Touch dry- 30 minutes at 30◦ C & 60 ± 5% R.H
Recoating After an interval of 4 hours
Finish Smooth Matt
Shade As per shade card
Shelf Life 1 year in closed container
PRECAUTIONS:
-
Do not apply putty or cement primers on exterior walls. Cracks can be filled with white cement or mixture of cement and sand if necessary.
-
Do not over thin the paint. Over dilution of Ocean Acrylic Exterior Emulsion may result in shade variation, poor hiding, poor bonding and flaking.
-
Do not use any universal strainers or other colourants.
COVERAGE CAPACITY:
FIRE HAZARD CLASS
Non- flammable
SAFETY MEASURES
Recommended to wear protective
clothing like gloves, overall, etc.